| Series | Al | Fe | Ca | Mg | Ti | Cu | B | K | Na | Li | OH |
| NC-200 | 18.00 | 0.40 | 0.50 | 0.05 | 1.15 | 0.01 | 0.20 | 0.80 | 0.90 | 1.20 | 120~260 |
| NC-210 | 15.00 | 0.20 | 0.40 | 0.05 | 1.20 | 0.02 | 0.10 | 0.60 | 0.80 | 0.40 | 120~200 |
| Series | Al | Fe | Ca | Mg | Cu | K | Na | Li |
| NC-W00 | 25.00 | 0.50 | 0.80 | 0.10 | 0.10 | 1.60 | 2.20 | 0.30 |
| Wavelength(nm) | 400 | 500 | 600 | 700 |
| Transmission | 1.0% | 1.2% | 1.2% | 1.2% |
| Series | Al | Fe | Ca | Mg | Ti | Cu | B | K | Na | Li | OH |
| NC-H00 | 14.00 | 0.40 | 0.50 | 0.05 | 1.20 | 0.01 | 0.10 | 0.35 | 0.70 | 0.80 | <5 |
| NC-H01 | 8.00 | 0.20 | 0.70 | 0.04 | 1.20 | 0.01 | 0.10 | 0.20 | 0.60 | 0.50 | <5 |
| Series | Bubbles mm | Homoge neity *10-6 | Striae | Birefringence nm/cm |
| NC-H00/101 | <0.1 | <15 | 1D | <15 |
| Series | Al | Fe | Ca | Mg | Ti | Cu | B | K | Na | Li | Mn | Ni | Co | Total |
| NC-S00 | 18.50 | 0.60 | 0.50 | 0.05 | 1.15 | 0.01 | 0.20 | 1.50 | 2.00 | 1.50 | 0.01 | 0.02 | 0.01 | 26.05 |
| NC-S01 | 14.00 | 0.59 | 1.00 | 0.15 | 0.79 | 0.22 | 0.06 | 0.70 | 1.50 | 0.80 | 0.01 | 0.02 | 0.01 | 19.85 |
| NC-S02 | 13.20 | 0.59 | 0.80 | 0.15 | 0.79 | 0.22 | 0.06 | 0.70 | 1.50 | 0.80 | 0.01 | 0.02 | 0.01 | 18.85 |
| NC-S10 | 0.07 | 0.11 | 0.02 | 0.01 | 0.01 | 0.01 | 0.01 | 0.03 | 0.03 | 0.01 | 0.01 | 0.01 | 0.01 | 0.34 |
| Property | NC-100 | NC-110 | NC-200 | NC-300 / NC-H00 |
| Density g/cm2 | 2.20 | 2.20 | 2.21 | 2.22 |
| Hardness KHN100 | 570 | 580 | 580 | 585 |
| Tensile *107Pa(N/m2) | 4.8 | 4.9 | 4.9 | 5.0 |
| Compression *109Pa | 1.1 | 1.1 | 1.1 | 1.1 |
| CTE(20-300ºC) *10-7/ºC | 5.5 | 5.5 | 5.5 | 5.5 |
| Thermal Conductivity(20ºC) W/mºC | 1.4 | 1.4 | 1.4 | 1.4 |
| Specific Heat(20ºC) J/kgºC | 660 | 670 | 680 | 680 |
| Softening Point ºC | 1630 | 1680 | 1690 | 1700 |
| Annealing Point ºC | 1180 | 1215 | 1210 | 1220 |
| Series | Density | Compression | CTE(20-300ºC) | Thermal Conductivity | Specific Heat | Softening Point | Annealing Point |
| NC-U300 NC-U400 |
1.95g/cm3 | >1.0*109Pa | 5.4*10-7/ºC | 1.1W/ºC.m | 650J/kgºC | 1600ºC | 1100ºC |